I fully charged the batteries and the resting voltage was about 80 volts. After about 10 km Under full load from a stop voltage was 72 and after 20 km full load voltage was 68 after 30km full load was 65.5. Resting voltage was always above 72. After 40 km battery was dead and resting voltage was 70 and 63.5 under full load.
It was 8 degrees Celsius. Just wondering about condition of batteries compared to when new. They are 72 volt 30amp hour lead acid. Thanks.