wb9k
10 kW
I have managed to get in contact with folks at OCSiAl, and today three gentlemen from the company came to Livonia to make a presentation and discuss possible applications. These guys have been quite helpful, and even mixed up some grease for us to experiment with here. They used Loctite 8104 mixed with 0.1% SWCNT's by weight. They used a high speed ball mixer to combine the materials and were very clear that this is the proper way to mix these types of materials together. More conventional/manual mixing methods result in agglomeration of the carbon, and performance apparently suffers for it. I will be trying some high current tests in the next week or so using both the grease they prepared, and what I have prepared previously. I'm curious how much difference the mixing method really makes. They showed us results where they stuffed a plastic tube with the grease and measured resistance through 1 cm of material. It was about 10 Ohms/cm in that arrangement. They're shopping this stuff pretty hard as a cathode powder additive as well.