townunheardof
1 mW
Hi again electric horsemen,
After two months away, I'm back to trying to troubleshoot my setup, which is a...
Cammy_cc 48v 15ah lifepo4 (new)
WE brushless 36v kit (2005)
IN the intervening time, I moved, had an operation, travel, vacation, battled bird mites from hell, all kinds of interruptions.
Here's where we covered some of this before http://endless-sphere.com/forums/viewtopic.php?f=2&t=9882
So, to sum up, when I start to ride, the controller cuts off. I don't think it has time to actually overheat much. If I keep the throttle low, I can go a little longer. But it cuts out whenever there's a substantial load. Mainly on uphills. It's a hair trigger. I never get much more than 1/8 of a mile or so before the controller shuts off, and I have to stop, turn it off, and turn it back on. My commute is 12 miles, so I'd have to stop and start like, 38 times to get to work.
I can't workaround this, somehow I have to fix it.
Some consensus seemed to say that I probably have a bad battery cell, or a "runt". I think this is probably the case.
I did figure out how to measure my voltage. I'm getting 50.3 V.
From what I gather, that's low, right? There's probably a runt in there because it should be 52 or 53.
So now I've got to take this thing apart? Find the runt? And replace the cell?
Now I realize, I never should have bought a Cammy_cc. I don't have the technical chops for this.
When my Charger self destructed, Cammy told me to send it back. $80 for shipping? Forget about it. For $80 I can probably buy a very good charger on Ebay or online somewhere.
I'm charging it now with my original WE 3 Amp charger, which seems to work fine.
I'm going to write to Cammy and ask him if he'll replace a faulty cell if I find one.
Maybe if I just keep charging and discharging over and over it will smoothe out and start working right...
Town
(SLA commuter for 3+ years, and not really interested in becoming a Lithium Tech)
After two months away, I'm back to trying to troubleshoot my setup, which is a...
Cammy_cc 48v 15ah lifepo4 (new)
WE brushless 36v kit (2005)
IN the intervening time, I moved, had an operation, travel, vacation, battled bird mites from hell, all kinds of interruptions.
Here's where we covered some of this before http://endless-sphere.com/forums/viewtopic.php?f=2&t=9882
So, to sum up, when I start to ride, the controller cuts off. I don't think it has time to actually overheat much. If I keep the throttle low, I can go a little longer. But it cuts out whenever there's a substantial load. Mainly on uphills. It's a hair trigger. I never get much more than 1/8 of a mile or so before the controller shuts off, and I have to stop, turn it off, and turn it back on. My commute is 12 miles, so I'd have to stop and start like, 38 times to get to work.
I can't workaround this, somehow I have to fix it.
Some consensus seemed to say that I probably have a bad battery cell, or a "runt". I think this is probably the case.
I did figure out how to measure my voltage. I'm getting 50.3 V.
From what I gather, that's low, right? There's probably a runt in there because it should be 52 or 53.
So now I've got to take this thing apart? Find the runt? And replace the cell?
Now I realize, I never should have bought a Cammy_cc. I don't have the technical chops for this.
When my Charger self destructed, Cammy told me to send it back. $80 for shipping? Forget about it. For $80 I can probably buy a very good charger on Ebay or online somewhere.
I'm charging it now with my original WE 3 Amp charger, which seems to work fine.
I'm going to write to Cammy and ask him if he'll replace a faulty cell if I find one.
Maybe if I just keep charging and discharging over and over it will smoothe out and start working right...
Town
(SLA commuter for 3+ years, and not really interested in becoming a Lithium Tech)