Did you guys see the announcement about the 2 men at MIT that have discovered a way to make a lithium battery that can be charged in 9 seconds ! I saw this on electricbikee.com
Here is another review ... that has some interesting points... such as the test samples... have only shown to increase discharge times ... it is hoped that they will 'could' also help reduce charge times... but that is not the scientific claim... and has not yet been tested or shown.
or forget the 2nd hand "translated" version... it the actual report from the actual scientists that did the work:
Here is the abstract the reporters baised their articles on:
which only talks about discharge rates... they haven't been able to get it to work at all for faster charge rates... notice how all the reports use the word 'could' when they describe the fast charging.... kind of like ... a cold fusion device 'could' power your house.
They got a massive 5 hour charge rate until 4.3V then holding 4.3V until current dropped bellow c/60.... yeah... that's an amazing 6+ hours charge rate. ... it will revolutionize ... oh wait... that isn't a revolutionary charge rate at all.
Considering that they only got 50mAh out of their test cell when discharging it in 9 seconds... compared to the same type of cell giving 170 mAh at a 2C discharge rate... yeah... it needs allot of work... as long as this reduces the batteries capacity to less than 1/3 of what it would be normally.... and of course they have yet to get it to work in the other direction , to charge the battery... as they have only managed to yet get it to work for discharging.