TerrySavace
🔌 New-ish
- Joined
- Feb 4, 2021
- Messages
- 41
Hi all,
I managed to obtain 200 unused "new" cells quite cheap (£1.20 each) so I have decided to undertake a battery build for my surron. They are Samsung 25r 20A 2500AH cells. They had been previously spot welded but all previous nickel removed. They were originally purchased from fogstar in the UK so are genuine.
I have tested each battery with a volt meter and they are all 3.50 volts bang on. If I manage to build this battery, I will prob go ahead and build a 42AH battery with 21700's. Thought id document it on here for others as i couldnt find anything on the net dedicated to building surron batteries DIY style! I also have a few questions for the community on here! Please dont judge me too much, my experience before under taking this has been limited to FPV drones
I also will be using an ANT BMS 20s 300A.
Batteries:

Building these into a 20s10p configuration, battery should give 200AMPs - around 2.1KW of power (very close to the stock surron battery KW)
Comparison of stock battery and my 72v battery stats:
STOCK BATTERY STATS:

MY BATTERY STATS:

I am attempting to make a battery like this : https://litespeedbikes.mybigcommerce.com/72v30ah-surron-drop-in/ I have basically read the description and trying to mirror that. I have also ordered a bac8000 from them and the egg rider and awaiting that to arrive.
Parts list so far:
Purchased these pure nickel strips 0.15x8x100mm
https://amzn.to/31kKpkS

This Tape - Accessotech 100ft Heat Resistant High Temperature Polyimide Tape Hot for Masking Soldering
https://amzn.to/3rrnazT

This spot welder
https://amzn.to/3rn5ZQ3

These Battery Insulator Rings:
https://amzn.to/2NSoNZP

These Foam sheets for eventually padding the battery out
https://amzn.to/2PrgKUr
Also ordered some of this to insulate the batter after build: "120mm 18650 Battery Insulation Gasket Paper Li-ion Cell Insulating Patch Pad"

I intend to create two external cables - one for powering the surron and one xt60 type of connection. I have ordered these connectors for powering the surron (will build another power cable for the surron) "Black Anti Spark Connector Male And Female QS8 High Current"

I have 3d printed the 18650 cell holders on a small printer - hence they are made up of multiple parts
The spot welder from amazon, seems to be doing the job and making decent welds
I have triple stacked the nickel in some places as per the photos
Current Build status:









So - as you can see, I have one half almost fully spot welded. I'm leaving each end off as I intend to solder the cables for -/+ and connecting the two halves to the nickel before spot welding it to the batteries.
My cable plan taken directly from the lite speed website on their battery https://litespeedbikes.mybigcommerce.com/72v30ah-surron-drop-in/ - if any experts can suggest any different let me know!!
I will be buying 12 AWG wire, and using 6 of them to connect each 1/2 of the battery.
I will be buying 10 AWG wire and running 3 of them off of the main positive side battery and splicing into 8 AWG wire for the surron positive load connection load - which will connect via the QS8 plug (AKA OSE-8)
I will use 3x10 AWG wires on the negative side to connect to the BMS, then from the BMS to the 8 AWG wire to the QS8 plug.
I will also connect some 10 AWG wires with an XT60 to the positive and negatives for charging. I am awaiting a 10A 72V charger purchased from www.electroncycles.co.uk in the UK.
Question i have is could i use copper butt connectors to "splice" the 3 10AWG into the 8AWG Main Load wires & charger cables? If so what ones shall i use? I have done some digging and i cant see any are rated for high enough AMPs. Or shall i just solder the cables together? Or shall i crimp them together? I will obviously be soldering the XT60 & OS8 onto the ends of each cable, just wondering the best way to connect / splice the actual wires together.
After this, I still need to figure out a way to build a case and fit the BAC8000 & egg rider!!
If you have read this far your a king, if you help me out - your a god!
have a good day people, hopefully I dont blow myself up!
I managed to obtain 200 unused "new" cells quite cheap (£1.20 each) so I have decided to undertake a battery build for my surron. They are Samsung 25r 20A 2500AH cells. They had been previously spot welded but all previous nickel removed. They were originally purchased from fogstar in the UK so are genuine.
I have tested each battery with a volt meter and they are all 3.50 volts bang on. If I manage to build this battery, I will prob go ahead and build a 42AH battery with 21700's. Thought id document it on here for others as i couldnt find anything on the net dedicated to building surron batteries DIY style! I also have a few questions for the community on here! Please dont judge me too much, my experience before under taking this has been limited to FPV drones
I also will be using an ANT BMS 20s 300A.
Batteries:

Building these into a 20s10p configuration, battery should give 200AMPs - around 2.1KW of power (very close to the stock surron battery KW)
Comparison of stock battery and my 72v battery stats:
STOCK BATTERY STATS:

MY BATTERY STATS:

I am attempting to make a battery like this : https://litespeedbikes.mybigcommerce.com/72v30ah-surron-drop-in/ I have basically read the description and trying to mirror that. I have also ordered a bac8000 from them and the egg rider and awaiting that to arrive.
Parts list so far:
Purchased these pure nickel strips 0.15x8x100mm
https://amzn.to/31kKpkS

This Tape - Accessotech 100ft Heat Resistant High Temperature Polyimide Tape Hot for Masking Soldering
https://amzn.to/3rrnazT

This spot welder
https://amzn.to/3rn5ZQ3

These Battery Insulator Rings:
https://amzn.to/2NSoNZP

These Foam sheets for eventually padding the battery out
https://amzn.to/2PrgKUr
Also ordered some of this to insulate the batter after build: "120mm 18650 Battery Insulation Gasket Paper Li-ion Cell Insulating Patch Pad"

I intend to create two external cables - one for powering the surron and one xt60 type of connection. I have ordered these connectors for powering the surron (will build another power cable for the surron) "Black Anti Spark Connector Male And Female QS8 High Current"

I have 3d printed the 18650 cell holders on a small printer - hence they are made up of multiple parts
The spot welder from amazon, seems to be doing the job and making decent welds
I have triple stacked the nickel in some places as per the photos
Current Build status:









So - as you can see, I have one half almost fully spot welded. I'm leaving each end off as I intend to solder the cables for -/+ and connecting the two halves to the nickel before spot welding it to the batteries.
My cable plan taken directly from the lite speed website on their battery https://litespeedbikes.mybigcommerce.com/72v30ah-surron-drop-in/ - if any experts can suggest any different let me know!!
I will be buying 12 AWG wire, and using 6 of them to connect each 1/2 of the battery.
I will be buying 10 AWG wire and running 3 of them off of the main positive side battery and splicing into 8 AWG wire for the surron positive load connection load - which will connect via the QS8 plug (AKA OSE-8)
I will use 3x10 AWG wires on the negative side to connect to the BMS, then from the BMS to the 8 AWG wire to the QS8 plug.
I will also connect some 10 AWG wires with an XT60 to the positive and negatives for charging. I am awaiting a 10A 72V charger purchased from www.electroncycles.co.uk in the UK.
Question i have is could i use copper butt connectors to "splice" the 3 10AWG into the 8AWG Main Load wires & charger cables? If so what ones shall i use? I have done some digging and i cant see any are rated for high enough AMPs. Or shall i just solder the cables together? Or shall i crimp them together? I will obviously be soldering the XT60 & OS8 onto the ends of each cable, just wondering the best way to connect / splice the actual wires together.
After this, I still need to figure out a way to build a case and fit the BAC8000 & egg rider!!
If you have read this far your a king, if you help me out - your a god!
have a good day people, hopefully I dont blow myself up!