Guys, I got 3A charger supplied with Frey EX. Checked output current, it's under 3A. Battery goes from 5% to 100% in 3 hours. Meaning it's accepted about 9 a/h of charge. But spec suggest 14a/h batteries. Max voltage suggest they are 100% charged to 4.2V, so no buffer at the top. I hear that there is some buffer at the bottom below 3.7V
Did anyone ever put battery thru capacity test? At face value, they appear overrated by 30%.
Same performance observed for in-tube and external battery.