HAL9000v2.0
10 kW
I have started with "Grayborg line" some 7 years ago. First one (warp a) was a micro scooter with 24V 280W motor and 15Amp controller from accu dril. Made so small so it can fit behind seat in my Bertone X1/9. It has 2s 12V7Ah bat and a top speed 30km/h. Of course that on the picture is only frame and tyres, everything else moved to next project 
warp b,c and d was 3 versions of steer-by-wire ICE motrorbike that one day will become electric (Perm PGM 132 waiting for controller) Test drive of warp c ----> http://www.youtube.com/watch?v=c_2DAMiJjhU
e,f and finaly g was 3 versions of frame for e bike. I am ended with g after few km without rear suspension on f.
So, frame is made of 2 pieces 1,2mm CrMo steel bended on CNC machine and welded to form tube 73x155mm. Controller WAS untill few days ago 36-72V 20A Crystalyte. Now is dead and I am waiting for new 4110 to come :lol: One of the wires on thermal protection fell off and it was overheated. I do not understan why they didn't use PNP instead ov NPN (or Viceversa).
Motor is x 504 and I am more than happy with it. I have tested it on 108V 66A for 3minutes (Than 2 batteries were dead), top speed on 5% downhill was 106 km/h and on same road uphill 65km/h. Motor was slightly warm but SLA was boiling.
Batteries are 6s 12V9Ah SLA in standard mode and 8s 12v 9AH in faster mode.
Now some pictures.
On the end is sneak preview of version H - combinaton of d and g...
Warp a
F was never painted because I strip him off for next version.
36V and 72V key next to the cover with new core duo style cooler
Intel inside
Ready for 4110
Seat adjusment screw
torque arm and rear breake holder
warp b,c and d was 3 versions of steer-by-wire ICE motrorbike that one day will become electric (Perm PGM 132 waiting for controller) Test drive of warp c ----> http://www.youtube.com/watch?v=c_2DAMiJjhU
e,f and finaly g was 3 versions of frame for e bike. I am ended with g after few km without rear suspension on f.
So, frame is made of 2 pieces 1,2mm CrMo steel bended on CNC machine and welded to form tube 73x155mm. Controller WAS untill few days ago 36-72V 20A Crystalyte. Now is dead and I am waiting for new 4110 to come :lol: One of the wires on thermal protection fell off and it was overheated. I do not understan why they didn't use PNP instead ov NPN (or Viceversa).
Motor is x 504 and I am more than happy with it. I have tested it on 108V 66A for 3minutes (Than 2 batteries were dead), top speed on 5% downhill was 106 km/h and on same road uphill 65km/h. Motor was slightly warm but SLA was boiling.
Batteries are 6s 12V9Ah SLA in standard mode and 8s 12v 9AH in faster mode.
Now some pictures.
On the end is sneak preview of version H - combinaton of d and g...
Warp a



F was never painted because I strip him off for next version.




36V and 72V key next to the cover with new core duo style cooler


Intel inside

Ready for 4110

Seat adjusment screw

torque arm and rear breake holder