I've setup regen on my Green time controller using a reed switch and magnet mounted on my hydraulic brake calliper. It works great while pack voltage is below 58V. Above 58V, there is no regen. Can anyone tell me how to modify the controller to enable regen at around 60V?
I'm running a 14S8P 18650 (with BMU) in series with a 1S8P booster pack made of plastic cell holders to get 15S. I check the Boost pack periodically to ensure it's balanced with the other cells. Usually I Bulk charge the 15S around 60V.
This is the controller:

Reading the forums, i think regen stops working at higher voltages because the LVC on my controller is set too low for 15S (currently LVC=40V). I think LVC should be increased to around 15x3= 45V.
Is it just a matter of shorting the terminals marked 60V on the circuit board to increase LVC and improve the Regen? Is there any way of knowing what the LVC will be if I were to do this?
![20211102_012857[1].jpg 20211102_012857[1].jpg](https://endless-sphere.com/sphere/data/attachments/173/173343-a68b4f1ded8debc22bd23cce8bdc9a47.jpg)
The Tabs for 60, 64, 72, 80 V are currently not used on the board (no resistor or short)

I'm running a 14S8P 18650 (with BMU) in series with a 1S8P booster pack made of plastic cell holders to get 15S. I check the Boost pack periodically to ensure it's balanced with the other cells. Usually I Bulk charge the 15S around 60V.
This is the controller:

Reading the forums, i think regen stops working at higher voltages because the LVC on my controller is set too low for 15S (currently LVC=40V). I think LVC should be increased to around 15x3= 45V.
Is it just a matter of shorting the terminals marked 60V on the circuit board to increase LVC and improve the Regen? Is there any way of knowing what the LVC will be if I were to do this?
![20211102_012857[1].jpg 20211102_012857[1].jpg](https://endless-sphere.com/sphere/data/attachments/173/173343-a68b4f1ded8debc22bd23cce8bdc9a47.jpg)
The Tabs for 60, 64, 72, 80 V are currently not used on the board (no resistor or short)