Having a new battery built.....

Nvreloader

10 mW
Joined
Mar 5, 2022
Messages
22
Location
Western NV
I am looking for the required or mandatory spec's to have a battery built,
from these 2 battery builders, UPP and EM3 EV.

Some of the questions I have are this:
Which of the below spec's are REQUIRED for a good battery build.
(I know nothing about building a battery, or what is required.)

80 cells = 21700 cells = equals my 2 OEM Bikonit Wart Hog MD 750 battery's,

MY OEM LG 21700 battery has 39 cells/13 in series, 3 in parallel, 15ah/720wh,
x 2 battery's, 30A controller. (OEM spec's)

Do I get 48V or 52V with a quality 30/40/50A BMS? (OEM is 30A)
Quality of the BMS?
Advanced BMS System?
Balance BMS?
Intelligent Dual Battery Balancing Module?

Proper cell connections/What type?
Do I need any cell protection fusing?
Cell separation / type?
Temperature monitoring?
Pure Nickel/Brass/Copper connectors ?

Case/construction methods ?
I would like a triangle case with these maximum dimensions =
Top = 431mm, Bottom = 457mm, Side =177mm x 88mm thick/wide.
Hard or soft shell construction?
Multiple wide HD straps to support the weight etc.

What else should I ask about/for?

Your thoughts and suggestion...
Thank you,
Don
 