Hi , I got a headway pack maid of 24 series 2 parallel (a38120se) lifepo4 cells .
Yesterday , i got my new adjustable charger , its a Mastech dc powersupply HY10010EX .
I put the charger on the pack whitout the BMS at 87.6 volts ( 3.65 v for 24 series ) .
The charge was looking good , start at 6.5 amp and slowly going down .
6 amps , 5 , 4 ..... 1.5 and then noise " tock , tock " comming from the pack
Unplugged the charger right away and check all my cells .... OH NOOOO .
4 of them are f..k , i check the voltage on those ( 0.597 v )( 0.274 v )( 0.004 v )( 0.001 v )
I try to charge them individually , nothing work still the same , I gess i overcharge them :x
I try to charge the pack whit the BMS , the charger wont start .
(1) I never gona charge whitout the BMS again
(2) I need a good BMS whit leds for this pack
(3) Can i do someting before puting them on shelf , reminding me how dumm i can be ?
(4) I probally gona need to buy some new ones , where ???
Yesterday , i got my new adjustable charger , its a Mastech dc powersupply HY10010EX .
I put the charger on the pack whitout the BMS at 87.6 volts ( 3.65 v for 24 series ) .
The charge was looking good , start at 6.5 amp and slowly going down .
6 amps , 5 , 4 ..... 1.5 and then noise " tock , tock " comming from the pack

Unplugged the charger right away and check all my cells .... OH NOOOO .
4 of them are f..k , i check the voltage on those ( 0.597 v )( 0.274 v )( 0.004 v )( 0.001 v )
I try to charge them individually , nothing work still the same , I gess i overcharge them :x
I try to charge the pack whit the BMS , the charger wont start .
(1) I never gona charge whitout the BMS again
(2) I need a good BMS whit leds for this pack
(3) Can i do someting before puting them on shelf , reminding me how dumm i can be ?

(4) I probally gona need to buy some new ones , where ???