That washer increases the surface area that helps hold the motor on as opposed to just the round axle. You could use a thinner one or dish the wheel with spoke adjustments to recenter it. Do you have v-brakes? If you have a disc a small bit of off center won't matter much. If V-brakes you should try to center the motor wheel.
otherDoc
Oh that is the front wheel and does have a disc. I guess you will have to adjust the spokes for centering. It is like dishing the rear wheel only in the front. You could run it a mm or two off center without a problem.
 
some progres:
front light alu housing (hi:3x ssc p4, lo:25x 5mm led)
rear light alu housing (6x 5mm led)
power meter alu/carbon housing with hobby king power meter and two switches for lights
 

Attachments

  • 17012013(002).jpg
    17012013(002).jpg
    383.5 KB · Views: 2,358
  • ostalo 412 (Small).jpg
    ostalo 412 (Small).jpg
    30.8 KB · Views: 2,358
  • ostalo 414 (Small).jpg
    ostalo 414 (Small).jpg
    29.4 KB · Views: 2,358
  • ostalo 417 (Small).jpg
    ostalo 417 (Small).jpg
    18.4 KB · Views: 2,358
  • ostalo 418 (Small).jpg
    ostalo 418 (Small).jpg
    19.3 KB · Views: 2,358
Sweet bike!

Your front light alu housing, is that something you made yourself or is it bought? Any more pictures of it?
 
bjosta said:
Sweet bike!

Your front light alu housing, is that something you made yourself or is it bought? Any more pictures of it?

you have some on a first page of this topic. I will post some more when i get it back from painting
 
capo said:
you have some on a first page of this topic. I will post some more when i get it back from painting

Doh! Missed that post :oops:
Will you run the light on your main batteries or from a smaller pack? will the light housing hold the battery?
Yes please do post more photos when you have it back, it's almost exactly the design I had in mind, but I haven't see anything likes this available. I've been looking for an affordable motorbike headlight to transform but haven't found one with the "right" design yet. Any chance you'd consider making another one? :D
 
I will run it on a main battery through the control panel (dash board-power meter)where i have two watter resistant switch for hi/lo mode
 

Attachments

  • ostalo 419 (Small).jpg
    ostalo 419 (Small).jpg
    27 KB · Views: 2,290
  • ostalo 421 (Small).jpg
    ostalo 421 (Small).jpg
    25.4 KB · Views: 2,290
  • ostalo 422 (Small).jpg
    ostalo 422 (Small).jpg
    28 KB · Views: 2,290
  • ostalo 423 (Small).jpg
    ostalo 423 (Small).jpg
    37.7 KB · Views: 2,290
  • ostalo 425 (Small).jpg
    ostalo 425 (Small).jpg
    32.6 KB · Views: 2,290
  • ostalo 427 (Small).jpg
    ostalo 427 (Small).jpg
    25.7 KB · Views: 2,290
..... iam stil waiting for front disk brake, than i will put evrithing together
 

Attachments

  • prednja luc 2 (Small).jpg
    prednja luc 2 (Small).jpg
    38.7 KB · Views: 2,262
  • zadnja luc 3 (Small).jpg
    zadnja luc 3 (Small).jpg
    59.1 KB · Views: 2,262
I have one question for you guys:

I need to install battery wires(2x 10awg) from front to back of the bike. Because I would like to have as clean as possible build iam thinking to bore two hols (10 mm wide) in upper tube of the frame.

What do you think?

Or would be better like this one did(mounted under the tube)
 

Attachments

  • $T2eC16VHJHYE9nzpeDFwBQYPmTfrE!~~60_57 (Small).JPG
    $T2eC16VHJHYE9nzpeDFwBQYPmTfrE!~~60_57 (Small).JPG
    66 KB · Views: 2,108
today I connected power meter and lights:
 

Attachments

  • ostalo 475 (Small).jpg
    ostalo 475 (Small).jpg
    15.6 KB · Views: 2,048
  • ostalo 467 (Small).jpg
    ostalo 467 (Small).jpg
    67.8 KB · Views: 2,048
  • ostalo 472 (Small).jpg
    ostalo 472 (Small).jpg
    52.8 KB · Views: 2,048
next step is to buy battery, I'm thinking to buy this ones:
http://www.ev-power.eu/LiFePO4-small-cells/WINA-LiFePO4-Power-3-2V-15Ah-aluminium-case.html

and mount it under the seat in bag like this or something simular:
http://www.ebay.com/itm/Leather-Motorcycle-Fork-Round-Barrel-Tool-Bag-Studded-Accents-12-x-5-/121054696048?_trksid=p2047675.m1850&_trkparms=aid%3D222001%26algo%3DSIC.CURRENT%26ao%3D1%26asc%3D11%26meid%3D6304761030227841126%26pid%3D100011%26prg%3D1005%26rk%3D1%26sd%3D120770570118%26

any other suggestion about batteries?
 

Attachments

  • ostalo 476 (Small).jpg
    ostalo 476 (Small).jpg
    68 KB · Views: 2,048
  • ostalo 478 (Small).jpg
    ostalo 478 (Small).jpg
    67.6 KB · Views: 2,048
  • ostalo 482 (Small).jpg
    ostalo 482 (Small).jpg
    68.4 KB · Views: 2,048
Battery-s finally arrived, final cost was 290 eur for 16 x 10.000mah lifepo4. I also bought aluminum pipe 150x100x300mm for housing. Now iam just waiting for bms:
 

Attachments

  • batteries.jpg
    batteries.jpg
    40.4 KB · Views: 1,995
  • ostalo 500 (Small).jpg
    ostalo 500 (Small).jpg
    21 KB · Views: 1,995
  • ostalo 501 (Small).jpg
    ostalo 501 (Small).jpg
    23.4 KB · Views: 1,995
  • ostalo 502 (Small).jpg
    ostalo 502 (Small).jpg
    25.8 KB · Views: 1,995
help Iam not a designer. Which position si better looking-to the design of bike:
 

Attachments

  • 1 position.jpg
    1 position.jpg
    85.4 KB · Views: 1,923
  • 2 position.jpg
    2 position.jpg
    88.3 KB · Views: 1,923
  • 3 position.jpg
    3 position.jpg
    82.7 KB · Views: 1,923
  • position1-1.jpg
    position1-1.jpg
    55.5 KB · Views: 1,923
That is gorgeous work. For balance of the handling in the triangle should work best. It does look a bit better under the seat back. Since that bike has such great curves perhpas you can put it in the triangle and make a larger cover that conforms to the steel tubes in the middle? I'm not a designer either!
otherDoc
 
capo said:
help Iam not a designer. Which position si better looking-to the design of bike:

None of the above...

No offense but the square chunk seems quite outta place on that bike. Triangle is definitely best weight distro and maybe a cool formed body panel could blend the rectangle into that area of the frame?

Or, maybe a saddlebag arrangement?
 
ok, new design- chopper bag. Now I must wait for bms:
 

Attachments

  • ostalo 512 (Small).jpg
    ostalo 512 (Small).jpg
    65.6 KB · Views: 1,821
  • ostalo 513 (Small).jpg
    ostalo 513 (Small).jpg
    83.7 KB · Views: 1,821
  • ostalo 514 (Small).jpg
    ostalo 514 (Small).jpg
    68.7 KB · Views: 1,821
Just wanted to say that I think your bike is looking most excellent! The bag looks much better but remember, you are going to have to figure a way to secure it so it doesn't bounce and jiggle. Think about building a hard (wood, plastic, mettle) box inside the leather bag so you you have something to attach to. Then you are going to need to make a mount to secure it to your down stays and or seat tube by either drilling and putting in threaded inserts or using clamps.

Keep Posting!
 
Good looking bike.
The black leather (rounded) battery bag is much nicer than the square box.
 
some progress was made(I put together battery pack). Now Iam waiting for some alu parts to return from painting and the bike project will be finished
 

Attachments

  • ostalo 533 (Small).jpg
    ostalo 533 (Small).jpg
    32.3 KB · Views: 1,737
  • ostalo 522 (Small).jpg
    ostalo 522 (Small).jpg
    37.9 KB · Views: 1,736
  • ostalo 523 (Small).jpg
    ostalo 523 (Small).jpg
    26.5 KB · Views: 1,737
  • ostalo 534 (Small).jpg
    ostalo 534 (Small).jpg
    50.9 KB · Views: 1,737
I hope you read this thread about MAGICPIE 3
IS your's MAGICPIE 3 with internal controller?
so read about experiences here:
negative experiences
http://endless-sphere.com/forums/viewtopic.php?f=4&t=47068
 
miro13car said:
I hope you read this thread about MAGICPIE 3
IS your's MAGICPIE 3 with internal controller?
so read about experiences here:
negative experiences
http://endless-sphere.com/forums/viewtopic.php?f=4&t=47068

I hope it will work fine. I know three people in my neighborhood who use it every day and they dont have any problem with it. I chose MP3 because I want as clean as possible look.

This is my first (testing)project, my second one will be Ego kit in my full suspension bike
 
Back
Top