Ipace LG pack fires?

Hillhater

100 TW
Joined
Aug 3, 2010
Messages
13,080
Location
Sydney ..(Hilly part !) .. Australia/ Down under !
Is Jaguar IPace going to be another Bolt type LG pack issue ?
This is not the first IPace pack reported to have ignited whilst garaged..
https://electrek.co/2022/08/01/jaguar-i-pace-catches-fire-another-bolt-ev-battery-fire-situation/
 

Attachments

  • 566E97C9-ADFC-4741-A15C-B52D31FE0466.jpeg
    566E97C9-ADFC-4741-A15C-B52D31FE0466.jpeg
    376.9 KB · Views: 1,152
That guy was super lucky he was able to get it out of his garage before it burnt hid house down.

Jaguar should have issued a recall as they use the same cells as the Bolt. I hope somebody sues the hell out of them over this.

 

Attachments

  • 2022-10-16 14_33_01-Jaguar I-Pace catches on fire again – is this another Bolt EV battery fire...png
    2022-10-16 14_33_01-Jaguar I-Pace catches on fire again – is this another Bolt EV battery fire...png
    319.6 KB · Views: 808