Hello,
I've been pulling several 4s1p 5Ah hard case packs from hk apart. After soldering them in parallel groups I noticed one of the cells had a strange odour coming from it. Not very strong, but noticeable.
Is the cells gone bad? They where never hot, and hold capacity and voltage well.
They are already soldered together, I don't want to take them apart if not necessary :?
I've been pulling several 4s1p 5Ah hard case packs from hk apart. After soldering them in parallel groups I noticed one of the cells had a strange odour coming from it. Not very strong, but noticeable.
Is the cells gone bad? They where never hot, and hold capacity and voltage well.
They are already soldered together, I don't want to take them apart if not necessary :?