http://www.alibaba.com/product-gs/401934491/3_2V_530Ah_Super_High_capacity.html
Ok... Maybe it's a bit too big for Skateboards........
http://www.alibaba.com/product-gs/401934491/3_2V_530Ah_Super_High_capacity.html
Quick Details
Place of Origin: Guangdong China (Mainland) Brand Name: OEM Model Number: 3.2V530Ah
Type: LiFePO4 cell
Nominal Voltage: 3.2V
Size: 22x430x768mm
( for those metrically challenged thats: .86" x 17" x 30.25" )
Nominal Capacity: 530Ah
weight: 14kgs Color: silver
Type: cell Lifecycle: 2000 times
Packaging & Delivery
Packaging Detail: wooden box
Delivery Detail 25 - 30 days
Specifications
Apply to electric motorcycle, electric floor washer, electric skateboard, electric forklift, electric bus, etc..
1. Typical Capacity: 530Ah
2. Cell Outer Dimension: 22x430x768mm
3. Nominal Voltage: 3.2V
4. End Voltage: 2.5V
5. Charging Current (max.) : 1C(=530A)
6. Discharging Current (Max.) : 1C(=530A)
7: Working Temperature:
Discharge status: -20°C~ +60°C
Charge status: 0°C ~ +45°C
Storage status: -20°C ~ +45°C
8: Temperature character:
60ºC @ 0.2C: 98% capacity;
23ºC @ 0.2C: 100% capacity
-20ºC @ 0.2C: 75% capacity
9. Cell Internal Resistance: <1mΩ
10. Weight: 14kgs;