Nicoist said:yes, of course lifepo4 is better than SLA. but you might want to check if your battery really delivers the advertised Ah's.
(i once received a 14 instead of 20Ah pack)
btw: lau's tonyyan51 ebay-account just got deleted, and my cheap won auction is thus canceled as well. luckily i didn't make the payment yet. also i don't like the fact that lau uses 1000s of accounts and also has weird specs on his products so I decided not to buy from him (probably a wise decision) and will now head for a ping pack. i should have done so right from the start...
greetings
nicolai
I'm testing battery ah right now with my kettle which is drawing 5.6amp.. I will be testing voltage every 10 minutes... see you in 3 hours 8)