district9prawn
1 kW
I got my PD's from fasttech. Before I built them in a pack I measured them at 2600mah discharging at 3A from 4.15v to 2.8. So not 100% but not duds either. Seemed to be the right model going by the discharge curves online. But yeah, sorry to hear you only got 1500 out of yours.