in sept I ordered from china Shenzhen Honshaoshend a triangle battery 145SP 12.5 AH 52 Volt Samsung lion 25R
then I heard about bb03 new release so I waited. I just got the bike together in dec
I measured the batt volts 27.8v at main lead (xt90) 30.9 volts (way low )
at charger lead (xt60) 30.9 volts
I tried the charger they sent it is putting out 58.9 volts, fan never comes on, doesn't get warm
I bought a very nice charger at luna, it is putting out 58.9 volts, fan comes on for a second then shuts off.
I can measure battery volts with charger in, it is around 54 volts(main lead)
I suspect both chargers are fine.
the battery refuses to accept any charge (I suspect due to protective circuitry on the battery or charger)
Shenzhen Honghaosheng Electronics Co., Ltd.
they want me to measure how many amps are coming from the charger. how do I do this? I suspect it is 0 due to battery management system- I am not familiar with battery management system. I am also not familiar with what kind of low voltage protection on the charger or the battery, so any explination would be great!
what is going on? any tips? how do I measure how much amps is coming from the battery charger?
they are saying battery was perfect when shipped, I did leave it in the box for a few months, payed with pay pal this is my first e bike, I am an rc guy very familiar with lipo packs, never had a problem.
I should have bought from luna or other vendor, I will listen next time.
here are the q they had for me.
Hi Frants,
I have discuss with our enginner as your battery pack problem.
Please help to answer us below questions:
1. the battery pack if can normal charging?
2.Please tell me which conenctor you test? XT60 or XT90.
3.how much is the charging voltage?
4.how much is the charging current?
Our enginner will analise the situation.and try to help you deal with it.
then I heard about bb03 new release so I waited. I just got the bike together in dec
I measured the batt volts 27.8v at main lead (xt90) 30.9 volts (way low )
at charger lead (xt60) 30.9 volts
I tried the charger they sent it is putting out 58.9 volts, fan never comes on, doesn't get warm
I bought a very nice charger at luna, it is putting out 58.9 volts, fan comes on for a second then shuts off.
I can measure battery volts with charger in, it is around 54 volts(main lead)
I suspect both chargers are fine.
the battery refuses to accept any charge (I suspect due to protective circuitry on the battery or charger)
Shenzhen Honghaosheng Electronics Co., Ltd.
they want me to measure how many amps are coming from the charger. how do I do this? I suspect it is 0 due to battery management system- I am not familiar with battery management system. I am also not familiar with what kind of low voltage protection on the charger or the battery, so any explination would be great!
what is going on? any tips? how do I measure how much amps is coming from the battery charger?
they are saying battery was perfect when shipped, I did leave it in the box for a few months, payed with pay pal this is my first e bike, I am an rc guy very familiar with lipo packs, never had a problem.
I should have bought from luna or other vendor, I will listen next time.
here are the q they had for me.
Hi Frants,
I have discuss with our enginner as your battery pack problem.
Please help to answer us below questions:
1. the battery pack if can normal charging?
2.Please tell me which conenctor you test? XT60 or XT90.
3.how much is the charging voltage?
4.how much is the charging current?
Our enginner will analise the situation.and try to help you deal with it.