Okay So I have 3 Multistar 4s 10ah lipo packs and on the third one the sides are fatter than the others and for some reason Cell #1 was drained to 2.8v and all the other 3 cells were at 3.5 to 3.7v, any idea why the first cell drained too quicker than the others? Should I try to balance charge them too 100% all the way until it beeps cause last few days I've been in a rush and basically letting it off when it is charging at 0.5a left when it has put around 9000mah and 16.80v in it.