I've just had to repair two punctures (fine steel wire) on my hubmotor wheel. I managed to do this without removing the wheel, but one of the punctures was right on the seam of the tube.
I fear that a patch across a seam won't seal, so normally spend a while trying to sand it away without thining the adjacent rubber. Hand work and not very good.
Not having decent sandpaper to hand today I tried my normal safety shaving razor from the bathroom. It worked perfectly! In 10 seconds I had a perfectly flat repair area and no damage at all to the tube.
I just thought I'd share
Ant
I fear that a patch across a seam won't seal, so normally spend a while trying to sand it away without thining the adjacent rubber. Hand work and not very good.
Not having decent sandpaper to hand today I tried my normal safety shaving razor from the bathroom. It worked perfectly! In 10 seconds I had a perfectly flat repair area and no damage at all to the tube.
I just thought I'd share
Ant