Tiber said:Would the BAC2000 be sufficient? The 4000 is out of my price range for now.
I have a BAC8000 and a QS205. Personally I would not use less than a 4000, it really is pretty well matched for the QS205. The biggest reason I like having an 8000 over the 4000 is the phase amps-- I've got upgraded phasewires, statorade, and hubsinks on my QS205 and while 450 is a very respectable peak phase current there have been times when I've enjoyed being able to crank the phase amps to 600 and watch the douche-canoes in supercars stop showing off to gawk at the 'bicycle' that just outpaced their six-figure midlife crisis... or to show off acceleration when people ask about it. 8) Technically my QS205 saturates around 220 phase amps but I've noticed 450 amps is about the point at which I notice it starts heating up much faster. I've only used 600 in short bursts.
I use my open-source Pi display to switch between power profiles on the fly with a 3-position switch, honestly if it wasn't for that and my motor mods I'd probably have been better off with a BAC4000 and sticking to 450 phase. :thumb: