Actually, I did consider adding the Tenpower 50SG as a third contender alongside the Samsung 50S and the Lishen 50LE. I expect the 50SG to offer decent battery life, though not as good as the 50LE’s; on the other hand, it should be more widely available than the Lishen. ... But then the Reliance RH60 arrived.
 
Have you tested Linkdata P60B? Looks not bad with max 60A current and 6000mAh :)
Attatched a batch of 40 units of Linkdata 60P, for now just measured AC IR and mass, check it:

ac_ir_linkdata.jpegmass_linkdata.jpeg

Average ac ir: 4,25 mOhms (1khz measured 4 point)
Average mass: 69,55 gr

If you want some special test I could do it, for now I will test 0.2C capacity, qOCV, 30A CC discharge till 2,6V...
 
If you want some special test I could do it, for now I will test 0.2C capacity, qOCV, 30A CC discharge till 2,6V...

Thanks for the data. Could you do a discharge test and temperature graph according to different current values (for exemple 15A, 20A, 25, 30, 35, 40) down to 2.5V ?

This way, we can compare it with other cells that Mooch has tested like the 50XG
 
Uh, Reliance's website is not available anymore :(

It points straight to a 404.

This isn't good...
 
Thanks for the data. Could you do a discharge test and temperature graph according to different current values (for exemple 15A, 20A, 25, 30, 35, 40) down to 2.5V ?

This way, we can compare it with other cells that Mooch has tested like the 50XG

No doubt! I will be uploading the tests done to these Linkdata 60P, also Mooch has done tests on his Patreon and I will be personally subscribing to it for seeing the tests compared to new Reliance RS60...
 
Huh, are they going under or what? They're supposed to be at AABC Europe next week.
E. Website seems fine to me? It's this one right
Oh my, I didn't notice, but this website has been heavily made with LLMs, I can tell.
I much preferred the old website :(
 
Does someone has the datasheet of the Linkdata 60P ? I'm struggling to find it and find their website other than the Alibaba listings
 
Oh my, I didn't notice, but this website has been heavily made with LLMs, I can tell.