today I recoverd 100 cells from two ebike used batteries
cells included samsung 29E version 6
original rated 2900mAh and minimum 2850mAh
doin some precise tests check pictures:
https://ibb.co/LN0dpSG
test subject Samsung 29E version 6 from used ebike battery
https://ibb.co/NNDzjqq
3A discharge 2,797Ah and 36.4 celcius
https://ibb.co/qnVYGxb
5A discharge 2,805Ah at 46,4celsius
cells included samsung 29E version 6
original rated 2900mAh and minimum 2850mAh