Hi All!
Hello everyone!
I just signed up
I bought a E-MAX 120L (VMOTO) Black / Orange a few days ago. I Was very Happy. :lol: but....
After a few days of use, the first problems began:
I leave home with 100% batteries;
after a few kilometers (about 5 of which 3 at a constant maximum speed of 65 km / h), the scooter turns off (as if the side stand was inserted), and the display writes "scooter disabled";
I turn it off by turning the key off;
Wait a few moments and then restart the scooter;
the batteries mark residual charge 01% - KM residual 00 - but still 52.7V;
I try to start and the scooter works properly, but without display shows wrong charge of (lithium) batteries.
I come home and try to put it in charge; seems to be charging, but the voltage is not aligned with the percentage of battery charge.
Charge charge when it marks 25% (because batteries are at maximum voltage as if they were 100%)
I try to make a turn.
I do about 20 km but the display always shows 25% of residual charge and always 18Km remaining as when I left.
Any idea?
Thanks all
Hello everyone!
I just signed up
I bought a E-MAX 120L (VMOTO) Black / Orange a few days ago. I Was very Happy. :lol: but....
After a few days of use, the first problems began:
I leave home with 100% batteries;
after a few kilometers (about 5 of which 3 at a constant maximum speed of 65 km / h), the scooter turns off (as if the side stand was inserted), and the display writes "scooter disabled";
I turn it off by turning the key off;
Wait a few moments and then restart the scooter;
the batteries mark residual charge 01% - KM residual 00 - but still 52.7V;
I try to start and the scooter works properly, but without display shows wrong charge of (lithium) batteries.
I come home and try to put it in charge; seems to be charging, but the voltage is not aligned with the percentage of battery charge.
Charge charge when it marks 25% (because batteries are at maximum voltage as if they were 100%)
I try to make a turn.
I do about 20 km but the display always shows 25% of residual charge and always 18Km remaining as when I left.
Any idea?
Thanks all