I have been looking for a way to give my wife a better foot rest as the ones on the motorino xpn are a bit awkward for her to use so I found some used folding pedals and looked at the area and well came up with this

image.jpg
image.jpg


Used some aluminum flat stock 1/8 x 2 and got longer bolts m6 x 40mm
Used some jb weld to hold them into the holes
 
I wouldn't use 3mm x 50mm aluminum for a smallish child much less my wife, unless I caught her having an affair and had a big insurance policy on her. :twisted: Bend it up and down a few times and it will snap right off.
 
There is very little movement of the aluminum if it does break I will replace it with some band iron
As it is just to hold her feet for her and she does not use it for getting on the bike