noise
the trike gets noise from the motor cable at the axle over 3200 watts
the stiletto sometimes gets noise at 3500 watts
same batteries
both phaserunners both heavy gauge grin motor cable but the wires are a little tighter going through the trike/mxus axle than the stiletto/3540 motor
saw those rental bikes all over vancouver today.
gotta question
i hard wired this PR in
this new phaserunner wont turn on and off, stays on
auto tuned fine, no faults
i run 2 wire regen, i connected it black and blue
is it supposed to be black and blue or red and blue????
regen works when activated while riding but if i push the regen button with tire in air, it wants to go backwards, tries to keep bouncing backwards, release the button and virtual electronic freewheeling starts turning motor forward. tire should just stop
went for a quick test ride and a bad vibration goes through the battery box on take off????
no faults
regen is the only connection i might of done wrong
edit***
went reading the version 3- PR manual
with the new CA plug, i think its made for a ca3 and im running a ca2 on this bike
the default for the on/off is different on PR-V3
the regen is wired correct as far as i can tell
the vibration on starting off, might be able to get rid of that by changing the throttle ramp up rate from 50ms to 70ms
im thinking this PR is putting out more amps than the old one
i used my old settings
when setting up the virtual electronic freewheeling the old setting was 1.5amps for 1 rev/sec
had to lower it to 1.2amps with the new PR
i have a ca3 on the trike, if i can get rid of the shudder tomorrow then ill just swap the phaserunners between the 2 bikes so the PR3 is with the CA3 and the PR2 is with the CA2