Scooter no go. Diagnose problem to be dead batteries. There are two of these BW1235DC-NB

BW1235DC-NB Specifications
Took the 2 batteries to battery store. Battery guy tested them with a load tester that looks like this.

One battery was bad. Bad as in RED. Other one was week. Week as in YELLOW.
I have a brain storm! See a whole pallet of used batteries. See one the same size as my scooter battery. Ask battery guy if we could trade my dead battery for the one on his pallet. He says yes. Now I got this used battery.
DCM0035

Had a lot of fun with lead acid date codes. Here is a Interstate Battery date code chart.

Go home and test it .5V
Charge with my 6 amp car charger. Put scooter all back together. It works! 
Yesterday I get a call from Scooter Girl. Battery capacity is not so good. She can not travel as far as she did before this bad battery episode.
Need recommendations on new battery or batteries. 2 - 12V batteries are wired in series for 24V. The speed that this things goes now is plenty fast. Any faster and it would tip over when going around corners.

Scooter no go. Diagnose problem to be dead batteries. There are two of these BW1235DC-NB

BW1235DC-NB Specifications
Took the 2 batteries to battery store. Battery guy tested them with a load tester that looks like this.

One battery was bad. Bad as in RED. Other one was week. Week as in YELLOW.
I have a brain storm! See a whole pallet of used batteries. See one the same size as my scooter battery. Ask battery guy if we could trade my dead battery for the one on his pallet. He says yes. Now I got this used battery.
DCM0035

Had a lot of fun with lead acid date codes. Here is a Interstate Battery date code chart.

Go home and test it .5V
Yesterday I get a call from Scooter Girl. Battery capacity is not so good. She can not travel as far as she did before this bad battery episode.
Need recommendations on new battery or batteries. 2 - 12V batteries are wired in series for 24V. The speed that this things goes now is plenty fast. Any faster and it would tip over when going around corners.