One more comment regarding the 60XG. In my experience, out of the hundreds of different cell models Iโve tested, only a handful have shown significant improvement within a single model name. In other words, this is as much as we can expect from 60XG model. Anyway Tenpower releases a โtesting reportโ document for its models, it would confirm this parameter for us.