Normally each string going to the BMS should read somewhere between 2.0v and 4.0v.
My guess is that if you measure 19v; you are measuring many string at once.
Third graph of this page could be helpful : http://scriptasylum.com/rc_speed/lipo.html
EDIT: If this is the only way you can measure...