Search results

  1. jakun

    Mark W Mark2 build/butcher thread

    I was lucky to get an other new controller from china for scooters. It's made for 72Volts and it works well up to 95Volts. I used it some time at this voltages. But now i just tried to connect 3 Dewalt batteries in series to it and it workes. The controller gets pretty hot @108V but it works. I...
  2. jakun

    Mark W Mark2 build/butcher thread

    Hi apropo destroying things. Here you can see what happens when full 30 Amrere goes into a dewalt Batterypack because of a dry joint in a double pack. I think some of the batteries just broke down and then the other got too high voltage and burst.
  3. jakun

    why does generic motor jam on crystalyte contoller?

    Hi I bought a new controller for higher voltage and cause the motor didn't run well I triet to do as you explained. Now it works well. But another thing that I detected is, that with an other hallsensor configuration than that which I am running now, the motor was verrry verrrry fast and did...
  4. jakun

    Your Creation's Before & After Pics

    Here is my new E-bike conversion. The only thing on my to do list is to install a disc brake on the front wheel.
  5. jakun

    Mark W Mark2 build/butcher thread

    The motor doesn't get really hot, just hand warm after a lng trip, but its winter here. I wonder how much I can push it. When I will do the 99V configuration, it will pull max. lets say 28Ax100V=2800W at acceleration and something between 1000-1500W at driving. It should got ca. 77Km/h freewheel...
  6. jakun

    Mark W Mark2 build/butcher thread

    you can just take a bigger batterypack. My is only ca. 4kg, so twise would be 8 kg with a range of up to 40km.
  7. jakun

    How do you charge your A123 cells...

    I do charge them first normally with 16A, so it's 4A per cell and when they are full, I plug in the ballancer to a pack after another to ballance if necessary. I ballance so, that the charger is still on. So the main volt level of the pack is allways the same, while ballancer is doing his job...
  8. jakun

    How do you charge your A123 cells...

    Hi here is how I charge my dewalt battery. I fond out, that it is ok to ballance the packs after a couple of charges. With this device I can charge the 2s2p pack in about 34-40 minutes when it's almost empty. The MRGN-900 gives 550Watt with (36V @16,2A) and I stick the 4 Dewalt batteries...
  9. jakun

    Mark W Mark2 build/butcher thread

    I drive my bike now for one month with nine continent brushless motor and this low cost controller from china: http://www.endless-sphere.com/forums/viewtopic.php?f=8&t=2615&p=42032#p42032 @ 4 dewalt 2s2p Akkupack and it rocks!!! I have a really good acceleration and a topspeed of 40 km/h. By...
  10. jakun

    Great charger/balancer combo for A123 also!

    I bought this thing and yes it does balance "stand alone".
  11. jakun

    Your Creation's Before & After Pics

    Hi, I've got it from ebay in germany. it's from gerda you can search for: "Gerda Touring Tresor Koffer schwarz 14 LITER" the guys name on ebay is: radwelt-hawner he has a shop.
  12. jakun

    Your Creation's Before & After Pics

    hi, no modifikation with the wattsup, it works just like this.
  13. jakun

    Puma/KMX trike at 82v A123

    Hi, I'm running a 48V 28A controller with 72V and a nine Continents Motor. Now I think about making a 3s2p Dewalt akkupack, whitch will be at ca. 105V. I thought about updating my controller with the 4110 mosfets and install new capacitors whitch will handle up to 100V(the actual ones are rated...
  14. jakun

    Collection of ebike pictures

    Hi volks! This is my first ebike, with a 60volt configuration. __________________________________________ Now upadted it to 72V with one more lead acid and now I have a top speed of 41km/h without paddeling. This rocks :lol: __________________________________________ Next project will be...
  15. jakun

    Your Creation's Before & After Pics

    Hi volks! This is my first ebike, with a 60volt configuration. __________________________________________ Now upadted it to 72V with one more lead acid and now I have a top speed of 41km/h without paddeling. This rocks :lol: __________________________________________ Next project will be...
  16. jakun

    Mark W Mark2 build/butcher thread

    hmm, and how does the gate driver look like? I think i found the gate resistors and they seem to be ok. here is another closeup picture of the controller. appendix: The controller works fine again.
  17. jakun

    Mark W Mark2 build/butcher thread

    You are right. I tried it and the motor problem was just the wires touching. Thanks . I ordered the other kit with the 48v controller and will try to compare them both and hopefully will find the problem with try and error.
  18. jakun

    Mark W Mark2 build/butcher thread

    here are the pictures, the wheel was unpluged , when the resistance occured.
  19. jakun

    Mark W Mark2 build/butcher thread

    Hi I have the same kit as you Mark and I burned my controller because of to high voltage ca. 73V :cry:. Now I'm waiting for a new one, but I realized another (problem?) When i turn the wheel (no power attached) only with hand, sometimes there is a big resistance, like something would be wrong...
  20. jakun

    Mark W Mark2 build/butcher thread

    Hi, i tested my wattsup and it shows up to 70volts, though it is rated to 60v