motosen said:
What do you think about
SUNringle MTX 33 and
Nimbus Dominator? ERD and width on first option should be fine but its not available anywhere at the moment. If second option has ~35mm inner width it could go with 2.4" tyre, I think. Though not sure about the ERD.
If the ERD is the same as your existing rim, then the same spoke length would work. If it's not, then you may have issues (there's a pic in one of those posts I linked that shows something from Sapim I think it is).
I haven't used the SunRingle MTX33 rim, but I have an old Sun Rhyno Lite I used on the front of SB Cruiser for some time, and it was used when I got it, and it held up well under various loads and impacts. I cant' remember for sure, but I think it was the wheel that was on the trike in it's only crash, where I broke the fork at the crowns but the wheel itself was intact. (IIRC I wore the hub bearing cups out and ended up replacing the wheel, saving the old one to relace later because I changed to disc brakes anyway).
I don't know if it would handle 12g nipples though, without drilling out the eyelets, which would defeat the engineering of the rim designed to make it strong. (same for any rim--if you modify it to fit something bigger than intended, it may fail because it's not made or used as-designed anymore).
Same for the Nimbus Dominator, on the nipple size and modification issues.
I will say that except for the lack of offset of the nipple holes, the Nimbus looks a lot like the rims I'm using on SB Cruiser on the rear wheels (where almost all the load is). Appearance doesn't necessarily mean anything, but if the source of the rims is that company, then they probably make good rims.
Both of those rims have been brougth up in various threads here on ES before, for strong rim suggestions:
https://endless-sphere.com/forums/search.php?keywords=sun*+mtx&terms=all&author=&sc=1&sf=all&sr=posts&sk=t&sd=d&st=0&ch=300&t=0&submit=Search
https://endless-sphere.com/forums/search.php?keywords=nimbus+dominator&terms=all&author=&sc=1&sf=all&sr=posts&sk=t&sd=d&st=0&ch=300&t=0&submit=Search