Compared to the ZEV4100 with the advanced Lithium batteries:
• The Lead is less expensive.
• Acceleration is slightly slower due both to the battery characteristics and the fact that the LA bike weighs approximately 145 kg / 319 lbs, which is approximately 24 kg / 53 lbs more than the lithium battery bike.
• Battery life is approximately 1/3rd as long as that of the lithium batteries. Expect about a 3.5 year life. However, they cost approximately only 1/3rd as much as the lithium batteries.
• Lead battery systems do not require battery management systems like the lithium battery. So that means a lot less parts to go wrong over time. This also means that the 4100 can be upgraded to a 5000 in the future with just a controller, one battery, and a new charger.
The Silicate lead battery used by ZEV are a completely different battery than the old lead sulfuric acid battery.
• They have only about 10% of the internal resistance of the old sulfuric acid battery. This allows these batteries to be charged in ½ the time of normal lead acid battery. • The discharge ability is much better allowing rapid vehicle acceleration with up to 4.5 times the ability to discharge without damage. • There is little or no temperature increases during charging or discharging. • The battery is far less sensitive to temperature being able to work normally at -50 C. • The battery has no memory. • The electrolyte is the ultimate green battery fluid as it can be used as a fertilizer. • The shelf life is in excess of 12 months without losing charge. So an unused vehicle does not run itself down. • The battery are non explosive. • The battery can be recharged at high currents of .8 to 1 C. • High discharge rates are not a problem given the low internal resistance. • There is not acid mist produced by charging. • The battery can be fully deep charged through over 500 cycles • The energy storage to weight ratio is about 24% better than lead acid.