Of course it will be "harder" than 7075 Al, and it will most likely wear better & last longer.
But stainless is not the best material for chainrings.
a flame hardened carbon steel would last even longer.
Looks like the teeth have the ends tore/worn off by a stretched chain. Best to change out the chain more often. Steel sprockets will last much longer, and oil helps also.
Many possibilities on ebay.