libbybikes
1 µW
- Joined
- Aug 18, 2022
- Messages
- 1
I installed the mid drive Bafang BBSO2 3 years ago with the 2V Turbocharge battery pack in 2019 & have used it off and on for commuting until June 2022 when it refused to turn on. I replaced the display with the new DPC-18 and now it will turn on for 5 minutes & shuts down for hours. I can power it up in the work stand after a few hours & the motor engages when I turn the crank, but if I walk it outside to ride, it shuts down & won’t come back for hours.