Peter Brigg
10 W
- Joined
- Jan 13, 2012
- Messages
- 90
I have made up a 12v battery using Headway 38120 10A cells -a pack of 8 cells with 4 pairs of cells in parallel to make what a charger sees as a 4cell 12v nominal voltage battery.
My idea was to have it as a General purpose 12v battery for camping and as an emergency starting battery for a 40 HP Yamaha outboard (but not to be charged by the outboard motor)
My only issue is with balancing the cells- the voltage readings currently for each of the paired cell s are- 3.41v 3.61v 3.37v 3.36v and this is after balancing and charging them with a Volt 680 AC multi function charger.
They were assembled with the proper metal connectors with all surfaces cleaned with fine sandpaper before fastening together.
There is a low voltage Zeva LVC12 cutout on the battery. Would you believe made in Australia.
The charger has many modes for these cells- eg balance,fast charge, storage and so on-all a bit complicated.
Plainly I am doing something wrong here.
Regards
Peter
My idea was to have it as a General purpose 12v battery for camping and as an emergency starting battery for a 40 HP Yamaha outboard (but not to be charged by the outboard motor)
My only issue is with balancing the cells- the voltage readings currently for each of the paired cell s are- 3.41v 3.61v 3.37v 3.36v and this is after balancing and charging them with a Volt 680 AC multi function charger.
They were assembled with the proper metal connectors with all surfaces cleaned with fine sandpaper before fastening together.
There is a low voltage Zeva LVC12 cutout on the battery. Would you believe made in Australia.
The charger has many modes for these cells- eg balance,fast charge, storage and so on-all a bit complicated.
Plainly I am doing something wrong here.
Regards
Peter