Hi, guys!
I'm trying to equip my catamaran with sun-electric motor setup. Motor will drain about 600 watts at maximum load (24V, 25 Amp), and my solar panel will produce around the same or even more power at full sun (will be about 4 square meters, 64s7p of 3*6 inch cells, 32V 25 Amps). Surely, I need battery to move when it's cloudy. I plan to charge it directly from solar panel.
I'd like to pay for battery not more than $400 including BMS. Endless-sphere online market offers different types of relatively cheap used batteries, and I need an advise - which choice will be cheaper?
What I need from battery:
1) 24V (or slightly above)
2) not less than 20 AH (the more the better)
3) discharge current 20-25 Amps, charge current 20-25 Amps
What I need from BMS:
1) Overcharge and overdischarge protection.
2) Overload protection (say, disconnecting at 50 Amps).
3) Charging control for CC-CV charging (PWM-based?)
3) Balancing - same voltage for cells in series.
What kind of cells are available:
1) Prismatic A123 3.3v 20Ah. I need 8 cells in series. The simplest case, the minimum weight, but not very cheap. Cells are $250.
2) Cylindrical 18650V, 3.7v 1.5Ah. I need 7 cells in series and, for example, 20 chains in parallel. It will give 24v 30Ah for about $200. But in this case I will need more complicated and more expensive BMS. Or not? I have read that there is no need for balancing this kind of cells. Is it true?
So, I need advice.
And another thing that I don't know - where should I search for appropriate BMS? May be somebody on E-S could make it for reasonable price?
I'm trying to equip my catamaran with sun-electric motor setup. Motor will drain about 600 watts at maximum load (24V, 25 Amp), and my solar panel will produce around the same or even more power at full sun (will be about 4 square meters, 64s7p of 3*6 inch cells, 32V 25 Amps). Surely, I need battery to move when it's cloudy. I plan to charge it directly from solar panel.
I'd like to pay for battery not more than $400 including BMS. Endless-sphere online market offers different types of relatively cheap used batteries, and I need an advise - which choice will be cheaper?
What I need from battery:
1) 24V (or slightly above)
2) not less than 20 AH (the more the better)
3) discharge current 20-25 Amps, charge current 20-25 Amps
What I need from BMS:
1) Overcharge and overdischarge protection.
2) Overload protection (say, disconnecting at 50 Amps).
3) Charging control for CC-CV charging (PWM-based?)
3) Balancing - same voltage for cells in series.
What kind of cells are available:
1) Prismatic A123 3.3v 20Ah. I need 8 cells in series. The simplest case, the minimum weight, but not very cheap. Cells are $250.
2) Cylindrical 18650V, 3.7v 1.5Ah. I need 7 cells in series and, for example, 20 chains in parallel. It will give 24v 30Ah for about $200. But in this case I will need more complicated and more expensive BMS. Or not? I have read that there is no need for balancing this kind of cells. Is it true?
So, I need advice.
And another thing that I don't know - where should I search for appropriate BMS? May be somebody on E-S could make it for reasonable price?