jasonf150
10 W
What does it mean when my positive batter connector (going from the battery to the controller) is melted together. It's not horrible, but enough to where I can't pull the connection apart. I can see where the plastic of the connector is melted a little.
52.8v, 9.2aH A123
40a 12fet controller (CA limited to 30a)
hs3540 motor
I ride 30 minutes twice a day, avg about 26mph. I stop pretty seldom thoughout that 30 minute ride, so I guess I ride it pretty hard, but I don't think I ride anywhere near as hard as some of the guys running closer to 100+amps. I got the battery from http://www.emissions-free.com and it does have the precharge (red/black/white wires) setup.
On a most-likely unrelated note, my chargers charge to a different voltage. I have one at work and one at home. When I leave my house in the morning, my cycle analyst reads ~55v, but after charging at work, it reads ~58v. Is that a problem? They are both 48v lifepo4 chargers which I also got from emissions-free.
Thanks for any help.
Jason
52.8v, 9.2aH A123
40a 12fet controller (CA limited to 30a)
hs3540 motor
I ride 30 minutes twice a day, avg about 26mph. I stop pretty seldom thoughout that 30 minute ride, so I guess I ride it pretty hard, but I don't think I ride anywhere near as hard as some of the guys running closer to 100+amps. I got the battery from http://www.emissions-free.com and it does have the precharge (red/black/white wires) setup.
On a most-likely unrelated note, my chargers charge to a different voltage. I have one at work and one at home. When I leave my house in the morning, my cycle analyst reads ~55v, but after charging at work, it reads ~58v. Is that a problem? They are both 48v lifepo4 chargers which I also got from emissions-free.
Thanks for any help.
Jason