Had a catastrophic failure on either the batteries or charger on my E-Grom this weekend :
Checked battery voltage on the bike and it was low, 66v, after sitting for the last month and a half. Plugged the charger in and it started charging. Usually it takes around 8 -10 hours to charge the pack (6 x 20ah lead acid). Checked on it after 8 hours and there was a smell like rotten egg coming from the bike. Quickly unplugged the charger (which was still charging), turned off the breaker switch, and moved the bike outside. Pulled the side fairing off of the bike and saw at least one battery was swelled. Next day took out all batteries and 4 were swelled up a lot, and the other 2 slightly. Checked the voltage on the charger when plugged in but not under load with a multimeter, and it read around 83.9v which seems correct. Took charger cover off and all looked fine, no blown components.
Does this seem like a charger or battery issue? I would guess bad battery if one or two were swelled but with all 6 swelled it seems like charger issue except charger shows its charging at correct voltage when I did the multimeter test.


Checked battery voltage on the bike and it was low, 66v, after sitting for the last month and a half. Plugged the charger in and it started charging. Usually it takes around 8 -10 hours to charge the pack (6 x 20ah lead acid). Checked on it after 8 hours and there was a smell like rotten egg coming from the bike. Quickly unplugged the charger (which was still charging), turned off the breaker switch, and moved the bike outside. Pulled the side fairing off of the bike and saw at least one battery was swelled. Next day took out all batteries and 4 were swelled up a lot, and the other 2 slightly. Checked the voltage on the charger when plugged in but not under load with a multimeter, and it read around 83.9v which seems correct. Took charger cover off and all looked fine, no blown components.
Does this seem like a charger or battery issue? I would guess bad battery if one or two were swelled but with all 6 swelled it seems like charger issue except charger shows its charging at correct voltage when I did the multimeter test.