• Hello ES! We could use some help to get us past the finish line on building the new knowledgebase for the forum.
    Can you donate? Please see our fundraising page. Thank you!

bluetooth BMS?

Thanksss!! :)
I am going to order same BMS for my Swytch kit, I want to replace the original dumb DMS with this one. Is there a sleep function for bluetooth or the sleep consumption is minimal?

How do I wire it for 10s battery?

The description says:

for 10S battery pack as sample , connect BC10-BC14 to battery cell 10# battery positive + .

Should the extra balance wires be connected (collected) to the last (like in the description) or the last but one series cell (like here).
 
Speaking of discharge switch function, does anyone know what voltage this switch circuit is operating at? Specifically for a JBD SP22S003B BMS. I am trying to figure out a resistor value for my LED indicator on/off switch.
 
Hi, I have this garbage BMS board, which went bad and totally drained my battery. These two mosfets circled in red are heating when the board is connected to the battery. Does anybody have some schematics so I can try to fix it, or should I throw it in the trash ?IMG_0314.jpg
 
Schematics are unlikely to exist. You'd probably have to trace everything out and draw them up yourself. :(

What number is on those parts to tell you they are mosfets? (knowing what part they are, you can replace them to see if that fixes it)

If they are simply being turned on by a faulty software or other hardware issue, it won't change anything, but if they are stuck on because they failed then replacing them will fix it. If you use parts with better specs than the originals, then it would be less likely to fail in that way again. (depends on the reason it did fail).



BTW, if your battery was truly totally drained (down to 0V? but even below safe cutoff levels is bad) then the cells are damaged and should be completely replaced*** not reused, so it's likely to be cheaper to buy a whole new battery with BMS than to do any repairs on this one.

***If you don't replace them, then the battery could fail catastrophically (fire, etc) at any moment in the future if a damaged cell fails in the wrong way. You cannot know if any cell is damaged this way until it does fail, and it's too late then. You can't predict whether or not it will fail this way, so it's not safe to reuse cells drained too far.

Fire is a low-chance but extremely high damage failure risk, so unless you're prepared to deal with the loss of everything (and everyone) involved in any fire that does happen, it's safer to not risk at all.
 