mistercrash
10 kW
What I used is thin cutting boards bought at the dollar store. The ones I got were something like 3 or 4 mm thick. The crazy carpet is an awesome solution too.
Teh Stork said:After charging; lower voltage means higher capacity.
999zip999 said:You can make 10p3s blocks for 12v and make a long string 6 blocks = 74v and have an extra 12v block for replacemant. Yes replacement. Or 21s for 86v. These are used cells.
999zip999 said:Charge blocks to 4.1v
Teh Stork said:Bottom line, if you have enough cells - you'll encounter a few weird ones.
pwbset said:I'm always amazed at the packs that are completely rusted... like did they leave them in the ocean or something? :lol: And the packs that have tons of crap in them like black soot or sawdust. It's amazing what gets in there.
Got any photos of your pack? My 18s10p triangle pack should be done by tonight after about 20hrs of labor. Hope I don't have any bad welds or anything anywhere.. was pretty thorough, but ya never know until you throw a few thousand watts through it.
Punx0r said:If you want to prevent movement between cells, would a string of hot glue not be a quick and easy solution when assembling the pack?
999zip999 said:pwbset I cut the overhang on the pos. end so it wouldn't touch the neg. case of the cell.
999zip999 said:I hooked the sense wires as 6s or 24v. and hooked a hyperion EOS pack sentry and bulked charged on a kingpan to 74.4v. But was having a lot of balance troubles difference cells random. So left it on the charger with sentries. I found that 5 and 6 cells where at 4.135v and the rest at 4.099v - 4.111v ? So balance with bulb without sentries and will see how they keep balance.
999zip999 said:Thanks once I like it's balance at 74.4v I will turn it up and balance 4.2v to see if they like it.