Sure, A123 battery from EM3 ev for the win. But also with better real world c rates than ping is any headway pack. So 15- 20 ah of headway will do. Or if you can carry it, add 10 ah more to your ping. 30 ah will do it for sure.
I'm also told that you can special order a pack from ping with 4c cells in it. That, which comes with the high amps bms, should run a 35 amps controller when you buy a 20 amps size.
Then there is RC lipo, where the crappy stuff is 20c, and it just goes up from there. Currently, since I couldn't afford a 48v 20 ah cellman A123 pack, I am running a 10 ah 48v lipo pack on everything. My old 48v 15 ah ping died, and my new big 5304 motor and controller on the longtail cargo bike are 40 amps.