Edge 1,500 with loose magnets and two broken need 10 magnets

999zip999

100 TW
Joined
Jan 10, 2010
Messages
11,846
Location
Dana Point So. Cal
I open up my 1,500 edge motor to find all but three magnets did not move. Yes I did get it hot. Blue the halls still work. I'm taking out the and have broken two so far. It doesn't seam to have any glue. ??? Still I will need two or more magents. Plus what glue ? Two part epoxy ? The magnets are 35.00mm x 13.60mm x 3.00mm
P.S I'm up to 4 broken magnets. They can fly away land and brake.
 
An epoxy they say you can fix an engine block will be high temp enough to glue back magnets, if you don't continue to cook off the motor. So JB weld, Pc7, etc is ok if you can't find really high temp epoxy.
 