DrkAngel
1 GW
.
Index Updated
I did the numbers on solar panel output, compared LiPo to SLA charging and discharging efficiency, rated usable cycle lives.
Showed LiPo needing about 60% the number of solar panels for the same provided electric return. - (through battery)
Showed 90% charged LiPo as cheaper than SLA in as little as 3 years. (cycled daily)
Received requests for all the 3s 1kWh packs I can build, SONY preferred!
3s50p 2.16Ah cell = ~1200mAh
Sorting through the ~1000 cells I charged last Fall, will only use those with negligible self-discharge and 6 packs of equally retained voltage.
Less than perfect cells to be used in inverter packs, or similar.
Perfect cells, gotta save the best ... reserved for my eBike builds.
Index Updated
Index Updated
DrkAngel said:.
.
. . . . . . . . . . . . . . . SONY LiPo Mapped!
Building my next battery packs using Sony LiPo.
I decided to precisely map charged capacity at specific voltages ...
These cells look excellent for prolonged usable life by reducing charged voltage!
These Sony cell lack the capacity bulge near 4.10V and will respond much more advantageously to charged voltage limitation! (I have in large quantity)
Differing cell formulations map very differently!
While I have never recommended charging specifically to 4.00V ...
(4.00V charge ~75% usable capacity x 400% usable lifespan)
$100 10Ah battery 3.70V - 4.20V (10 mile range x 500 cycles = 5000 mile lifespan)
$135 13.5Ah battery 3.70V - 4.00V (10 mile range x 2000 cycles = 20,000 mile lifespan)
(Looks to be an excellent bargain!)
I have often recommended charging specifically to 4.10V ...
(4.10V charge ~90% usable capacity x 200% usable lifespan)
$100 10Ah battery 3.70V - 4.20V (10 mile range x 500 cycles = 5000 mile lifespan)
$111 11.1Ah battery 3.70V - 4.10V (10 mile range x 1000 cycles = 10,000 mile lifespan)
Charging oven lower 3.95-3.90V looks very usable ... !
These cell look optimal for extreme long life for my mobility scooter (eTrike) builds. (NEV might be better, more descriptive)
At designed 10mph, 4.00V 500Wh battery should give 2000 ~25mile cycles = 50,000 miles
(These SONY cells have deteriorated minimally in their 6-10 year ageing, unused samples exhibit 90%+ of rated capacity! )
I did the numbers on solar panel output, compared LiPo to SLA charging and discharging efficiency, rated usable cycle lives.
Showed LiPo needing about 60% the number of solar panels for the same provided electric return. - (through battery)
Showed 90% charged LiPo as cheaper than SLA in as little as 3 years. (cycled daily)
Received requests for all the 3s 1kWh packs I can build, SONY preferred!
3s50p 2.16Ah cell = ~1200mAh
Sorting through the ~1000 cells I charged last Fall, will only use those with negligible self-discharge and 6 packs of equally retained voltage.
Less than perfect cells to be used in inverter packs, or similar.
Perfect cells, gotta save the best ... reserved for my eBike builds.
Index Updated