Hello electric bike community,
here is my project from Germany.
A Honda CRF 250 from 2017. With the conversion QS138 4000W 90 H and Votol EM 200/2
The battery is 72V and 90ah, the biggest I got in. When assembling the battery first had to go through the frame.
https://youtube.com/shorts/72BhGK6Qa4I?feature=share
https://youtube.com/shorts/xuaETIa2Mg8?feature=share
I've already done test drives, but I'm not entirely satisfied with the performance, I think it would do better..
My problem is that I cannot program the EM 200/2. Cannot connect to Windows 11 PC...
The Votol Bluetooth Adapter for Android does not give any plausible values either.
I bought the whole kit from Harry QS. He is very nice but always sends the same versions of the program and driver. Without solution.
Today, after the 3rd test drive and a break, the engine no longer starts, but you can hear humming noises and when I turn the engine by hand and give it the throttle, it runs.. see video.
https://youtube.com/shorts/Vb80TDg-bAE?feature=share
Can you help me? Does anyone know the problem?
Who also has an EM 200/2? I wanted the best but it seems more of a disaster.
What is the best controller for the QS138 4000W.
Greetings from Cologne.
Peter
here is my project from Germany.
A Honda CRF 250 from 2017. With the conversion QS138 4000W 90 H and Votol EM 200/2
The battery is 72V and 90ah, the biggest I got in. When assembling the battery first had to go through the frame.
https://youtube.com/shorts/72BhGK6Qa4I?feature=share
https://youtube.com/shorts/xuaETIa2Mg8?feature=share
I've already done test drives, but I'm not entirely satisfied with the performance, I think it would do better..
My problem is that I cannot program the EM 200/2. Cannot connect to Windows 11 PC...
The Votol Bluetooth Adapter for Android does not give any plausible values either.
I bought the whole kit from Harry QS. He is very nice but always sends the same versions of the program and driver. Without solution.
Today, after the 3rd test drive and a break, the engine no longer starts, but you can hear humming noises and when I turn the engine by hand and give it the throttle, it runs.. see video.
https://youtube.com/shorts/Vb80TDg-bAE?feature=share
Can you help me? Does anyone know the problem?
Who also has an EM 200/2? I wanted the best but it seems more of a disaster.
What is the best controller for the QS138 4000W.
Greetings from Cologne.