NeilP
1 GW
After waiting 4 weeks for it to arrive, I have just trashed a new 11-28 DNP Epoch freewheel
It has more metal at the back, behind the biggest cog, than my old freewheel so the biggest cog was a good 12mm away from the motor side cover, as opposed to 8mm on my old freewheel.
This is always the danger of starting a new job after midday..If you can't make a start on a job early morning..then give up and start the next day. I made a start on this at 3pm.
So since the back was too thick, I thought I'd spin a bit of extra metal off of it on the lathe. But I could not manage to get it to hold correctly, and going up to my mates to use a milling machine...nah..lets just use the 9 inch angle grinder.
What a f wit!! took too much off, over heated it and it is now gritty as hell and does to turn properly...No more than I expected really ...bloody idiot. Now I'll have to wait another 4 weeks for a new one to arrive from the USA ...
I left it as is for now...I may yet be able to take off the rear locking ring, and strip it...but it looks very much like I have taken too much off of the main body...pretty sure I can see a line ...like I am cutting through the edge of a supporting wall![Frown :( :(](data:image/gif;base64,R0lGODlhAQABAIAAAAAAAP///yH5BAEAAAAALAAAAAABAAEAAAIBRAA7)
It has more metal at the back, behind the biggest cog, than my old freewheel so the biggest cog was a good 12mm away from the motor side cover, as opposed to 8mm on my old freewheel.
This is always the danger of starting a new job after midday..If you can't make a start on a job early morning..then give up and start the next day. I made a start on this at 3pm.
So since the back was too thick, I thought I'd spin a bit of extra metal off of it on the lathe. But I could not manage to get it to hold correctly, and going up to my mates to use a milling machine...nah..lets just use the 9 inch angle grinder.
What a f wit!! took too much off, over heated it and it is now gritty as hell and does to turn properly...No more than I expected really ...bloody idiot. Now I'll have to wait another 4 weeks for a new one to arrive from the USA ...
I left it as is for now...I may yet be able to take off the rear locking ring, and strip it...but it looks very much like I have taken too much off of the main body...pretty sure I can see a line ...like I am cutting through the edge of a supporting wall