Hi Guys, I have two battery pack Prismatic LiFeP04 (15ah 24s) in parallel = 30ah 76.8 nominal. I use Cycle Satiator charger set to reach 86volt for charging my pack.
When the pack is full, the charger keep the pack fully charged.
When I unplug the charger, the voltage begin to drop slowly until 84v. This is normal or not? It is better to set the charger at 84v? instead of 86v? I not want to break my pack.
I tried without BMS and same thing.
thanks. 8)
When the pack is full, the charger keep the pack fully charged.
When I unplug the charger, the voltage begin to drop slowly until 84v. This is normal or not? It is better to set the charger at 84v? instead of 86v? I not want to break my pack.