Nice!
Are the smaller ones available in a case like the 100Ahr one?
Are the smaller ones available in a case like the 100Ahr one?
patrick_mahoney said:What does the calendar life look like - by which I mean, how long will the battery last if it just sits around? Early LiFePO4 batteries had impressively large cycle time counts, but not particularly impressive calendar/shelf life (<3 years). Is this still an issue?
Are these LiFePO4, or are they C-LiFePO4?
eP said:If you recharge them twice a day and discharge them at high rate so after 10 month they could be over.
So what is the difference if they have 2 or 3 calendar life years ?
10 months it is less than 2 bike's riding seasons.
Lowell said:eP said:If you recharge them twice a day and discharge them at high rate so after 10 month they could be over.
So what is the difference if they have 2 or 3 calendar life years ?
10 months it is less than 2 bike's riding seasons.
Like I said 'if you don't ride one bike all the time'
Some people have more than one vehicle![]()
safe said:Price, price, price?![]()
How much less ?aiicsu said:eP said:What is internal resistance for each pack and what are the burst current ability ?
What is the price per Ah ?
internal resistance is less than 150m ohm
aiicsu said:burst current ability is about 4c-5c
the price is base on burst current .
aiicsu said:it is about $2.3 per ah
Nominal Nominal Max Discharge Cycle Life Dimension Weight List Price
Voltage capacity Current (80%DOD) (mm) (Kg) US$
@ 0.3C (Continuous)
TS-LFP40AHA 3.2V 40AH 120A 1000 190x116x46 1.5kg $80
TS-LFP60AHA 3.2V 60AH 180A 1000 215x115x61 2.5kg $120
TS-LFP90AHA 3.2V 90AH 270A 1000 220x145x68 3.0kg $180
What would a 36 volt 12.5 ah pack with bms and charger costaiicsu said:my price is package price,not for single cell.eP said:aiicsu said:it is about $2.3 per ah
Is it competitive price to that ?
http://www.everspring.net/txt/product-battery-pricing.htm
Nominal Nominal Max Discharge Cycle Life Dimension Weight List Price
Voltage capacity Current (80%DOD) (mm) (Kg) US$
@ 0.3C (Continuous)
TS-LFP40AHA 3.2V 40AH 120A 1000 190x116x46 1.5kg $80
TS-LFP60AHA 3.2V 60AH 180A 1000 215x115x61 2.5kg $120
TS-LFP90AHA 3.2V 90AH 270A 1000 220x145x68 3.0kg $180
if you need single cell ,the price is less than $2.0
aiicsu said:my price is package price,not for single cell.eP said:aiicsu said:it is about $2.3 per ah
Is it competitive price to that ?
http://www.everspring.net/txt/product-battery-pricing.htm
Nominal Nominal Max Discharge Cycle Life Dimension Weight List Price
Voltage capacity Current (80%DOD) (mm) (Kg) US$
@ 0.3C (Continuous)
TS-LFP40AHA 3.2V 40AH 120A 1000 190x116x46 1.5kg $80
TS-LFP60AHA 3.2V 60AH 180A 1000 215x115x61 2.5kg $120
TS-LFP90AHA 3.2V 90AH 270A 1000 220x145x68 3.0kg $180
if you need single cell ,the price is less than $2.0
aiicsu said:LiFePO4 polymer battery for e-bike is avialable
it is polymer battery
the capacity is 5-200Ah
cycle life :>1000 times 75% initialization capacity (@0.5C charge and diacharge rate)
aiicsu said:it is 100% DoDeP said:aiicsu said:LiFePO4 polymer battery for e-bike is avialable
it is polymer battery
the capacity is 5-200Ah
cycle life :>1000 times 75% initialization capacity (@0.5C charge and diacharge rate)
1000+ times at what DoD ?
What would be shiping cost/ shiping time to Poland ?
Is this possible classify them as RC components (free of tax duty - in Poland ) ?
aiicsu said:it is 100% DoD
Aiicsu and anyone who is selling anything on the internet needs a web site. Go heremarty said:Aiicsu - Got a suggestion for you. Go here http://www.domain-website-hosting.com think they connected with http://www.godaddy.com Pay $3.99 a month and set up a simple web site. There are cheaper hosting companies, but these guys have 24 hour questions. List some complete lithium batteries with chargers, total prices, weight, size, electric info, and a picture or two. Look what I do http://www.voltev.com it only took about a hour. If you don't know how to make a web site, your kids will help you. I can help too.
aiicsu.com is available
marty said:Aiicsu and anyone who is selling anything on the internet needs a web site. Go heremarty said:Aiicsu - Got a suggestion for you. Go here http://www.domain-website-hosting.com think they connected with http://www.godaddy.com Pay $3.99 a month and set up a simple web site. There are cheaper hosting companies, but these guys have 24 hour questions. List some complete lithium batteries with chargers, total prices, weight, size, electric info, and a picture or two. Look what I do http://www.voltev.com it only took about a hour. If you don't know how to make a web site, your kids will help you. I can help too.
aiicsu.com is available
http://office.microsoft.com/en-us/office_live
FREE domain name
FREE Web site design tools
FREE 500 MB of Web site storage
FREE company-branded e-mail and instant messaging
FREE tool to manage your Windows Live Search keywords
FREE download of Office Accounting Express 2007
Think Bill Gates will get millions of people with credit cards to set up free web sites. Then charge them all $ That be millions of dollars!
eP,eP said:If he has right (competitive product) aimed at right target group the web site is not especially important.
If he has a competitive product aimed at right target group than he dont need advertise at all.marty said:eP,eP said:If he has right (competitive product) aimed at right target group the web site is not especially important.
Please recommend a better, lower cost way to advertise a product. Better then a free web site?