2+ year old 48v20ah ping. Over 10,000 miles. May have been overcharged to 4v a few times. Capacity un-tested in the last 12 months, but previously it was holding up fine.
NO BMS ON THIS BATTERY.
Sitting on my power supplies in storage, as in ready to ride when ever, at 3.6v per cell It goes out of balance after two weeks. 150mv deviation according to the cell logs. Some cells at 3.45v some at 3.65.
What causes this?
NO BMS ON THIS BATTERY.
Sitting on my power supplies in storage, as in ready to ride when ever, at 3.6v per cell It goes out of balance after two weeks. 150mv deviation according to the cell logs. Some cells at 3.45v some at 3.65.