Masini Extremo build scooter with >30kw

Today I reassembled my scooter.
The controller has a 18W Fan with a seperate temperature switch underneath the grey venting cover , to cool it on hot days.
The QS10 charge plug has now got an extra 150A fuse, because I do not want to have unfused wires running through my scooter.

I had to add a 3.3K resistor to the motor temperature wires because my controller has only KTY81-130 listed and my motor has kty83-122 installed. Now the values at 140C are identical and thermal protection does not cut power to early.

20240308_161602.jpg20240308_151415.jpg

The controller has another problem since I solved the mess in the ratios of speed. The regen does cut the throttle until the wheel stops completly. At my first testrides it worked perfect and the regen power was controlled with the throttle.
Now I have to turn off regen.

I need a new firmware.
 
Last edited:
First charging test with >1C 8.5-9.5kw
Battery stays cool.
I can raise up to 160A but my power cable to the garage is 40years old an can not handle more. You still see my not perfect connection to cell 11 and 21 with 55mV cell difference. Without charging current it was 6mV.
Screenshot_20240309_151923_BMS.jpg
 
Last edited:
The problem with the regen not letting go until the bike stoppes happened to me when it was setup wrong. There are 2 values to setup, one has to be bigger than the other. If that is wrong, this is what happens.
 
Thanks for the Info.
The lower is shown as 40A and the higher 60A.
Problem is the software does not let me change these values at the moment, so I can't try other values.
 
I sorted a few things. The App has let me change some values.
Brake and sidestand do now cut the motor.
Regen works now with the brakes.
Problem was the max Value had to be raised and the ratios had to be lowered.
The variable regen with the throttle does still not work. But i think the closed throttle has a wrong voltage value. I did tests on the main stand and with very less throttle the motor starts to spin and does not stop when the throttle is realesed, but the app does not let me change the value.

Some new measurements
0-100kp/h 1400pA 400bA
I let the controller reduce current above 95kp/h as I have fear killing my BMS uphill.

Screenshot_20240315_133258_GNSS PA.jpg

400bA are reached in less than 1.5 seconds.

Screenshot_20240315_135154_Gallery.jpg
 
I sorted a few things. The App has let me change some values.
Brake and sidestand do now cut the motor.
Regen works now with the brakes.
Problem was the max Value had to be raised and the ratios had to be lowered
Today it cut power two times with activated regen. Shown Error was "undervoltage" and the controller changed from "MTPA" to "weak" at around 350rpm after 2 seconds regen. Battery SOC was at 70% , so no reason for an undervoltage or overvoltage alarm.
I tried to raise stop back and max back values for 40/80A to 60/120A and during saving the controller changed the values to 4/6A and now the new App does not let me change the values.
I had to take my old phone with the 1.5.5 and change the values back , but I had to change to the new phone with the 2.4.9 to save the values.
That is still a big Ssoftware mess.
Next week I will try the Ios App.
 
One Issue could be found with cutting out regen. It is definitly not a controller problem.
My JK-BMS is cutting the regen current, when the battery is colder than set in the temperature setting, and then the controller gets in trouble when regen is activated. If it was a Sabvoton it would already be dead. But the Fradriver mangages and survives even this situation.

I set the undervoltage temperature in the BMS to 14C and the release to 14.1C, Problem is that it does not allow charging current under 14.1C but heating ist turned on at 14.0C. That is not how I wanted it to be. Before I had a seperate heating controller set to 14C and the BMS did cut charging at 0C. Probably I have lost my possibility to preheat my battery to a desired value for better performance.

I also have found a Firmware for the ND721800 in the internet.
Problem ist that I do not know if it fits my controller.
Firmware is ND721800_63_ARA24
Controller is ND721800_63_ARG15
 
Last edited:
New small charging setup
2x Flatpack S 1800W in series.
73x83x260mm or 41.5x146x260mm . 2kg max 37,5A
The Flatpacks are smaller, lighter and more quiet than my previous Vertiv R48-2000E3 setup. The Vertiv turn up their fans to nearly full speed under 48V even without load.
I still have to test what this Duo will do at 70V and I have to get a new plastic Cover, the one on the picture is from a previous Eltek Flatpack 2 HE Setup.
 

Attachments

  • 20240412_203614.jpg
    20240412_203614.jpg
    2.2 MB · Views: 14
  • Screenshot_20240412_203432_BMS.jpg
    Screenshot_20240412_203432_BMS.jpg
    522 KB · Views: 14
Last edited:
I'm still working on the can code for the delta 48V 3000W rectifier (the one on the left) which is only a little longer as the Vertiv R48-2000e3.
The Delta is 1.3kg at 3050W. The Vertiv .is 1.13kg and the Eltek on the right is 0.85kg. Two Delta in series with a 30V 3.2kw supply will make a 5kg three phase 9kw charger.
20240110_180452.jpg
 
Last edited:
Impressive machining to make the battery fit and widen the swingarm. impressive all around. I must say that I really like the colors as all of my builds are green, black, & white or silver. Thank you again for documenting & sharing the details. Upon successful reconfiguration with a far driver controller, larger battery and new front suspension, I will do the same. Peace & Blessing,
Erthsrvntxx
 
The Eltek Flatpack S Duo does not charge my battery when it is discharged to 70V. After a minute they turn off.
I have to find a Flatpack S 24V to bring this small charging Setup to work.

Meanwhile I also bought a few used Vertiv R48-1000E3.
IMG-20220928-WA0002.jpg
I had bought two new ones over two years ago, but did not want to solder on them, so I never tested them under load. Now I also found a compatiple plug for them.
With only 0,6kg and 41x52x152mm they are small and lightweight, the downside is, the do not accept permanent voltage settings under 48V.
 
Last edited:
Bought an Eltek Flatpack S Rack with 24V 1000W rectifiers and a smartpack Controller.
20241031_122244.jpg

I changed my Flatpack S charger to one 48V 1800W and a 24V 1000W connected in series. This makes nearly 2,7kw charging power from empty to full. All the voltage drop while charging my empty battery is done by the 48V Flatpack. Th2 24V only reduces its output voltage by 0,2V.
Screenshot_20241030_133640_BMS.jpgIMAGE_86baf3e4-a6f4-4e55-bf54-27406f43da7a.jpgIMAGE_f0c2cdcd-b584-417b-a707-d5433f3e1ed8.jpg
 
New JK-B2A-24S30P BMS has arrived. If it fits in my scooter, 500A from the battery could be achived, now I'm limited to 400A.

On the pics next to it the 20P Version which is installed in my scooter.
The new one has 300/600A.
The old one has 200/350A (the 350A can be drawn up to 60seconds and the cut off time can be set in the software)

20250409_160950.jpg20250409_161112.jpg
 
Worn tires and brake pads and the rear dampers, nothing else was changed during the last two years, I'm just driving.

Since an App update I can't get acces to the Fardriver Controller anymore, so I can't crank up line and phase amps, therefore the bigger BMS is still not installed.

I also did not finish my 120A three phase charger with 120A from empty to full battery, as there was no need for it.
I managed to set voltage and current on the Delta 3kW rectifiers, but I bought a new version from them with 98% efficiency and they don't not accept any changes.

A few weeks ago I wanted to buy two VW 6,85kWh 12S MEB Battery Modules to replace my battery with and get more then 45kW peak power, but the guy who sold four modules to a friend of mine at rhe other end of Germany didn't not respond to my Mails, and when I was in his City 400km away from me he had only one left.

The next thing will be a new and lighter battery, but there is no need for it at the moment.
Mine is extremly heavy, +70kg and now 7 years old, but still going strong. Internal resistance has raised a lot in the last two years, but it is still driveable.
I think it will last two more years before the resistance is to high for 400A.

I still want to make my own E-Motorcycle, but the ingeneer from TüV is not wiling to make it legal without a full emc test.
That would cost me half the price of a new Zero SR/F.
 
Last edited:
Since an App update I can't get acces to the Fardriver Controller anymore, so I can't crank up line and phase amps, therefore the bigger BMS is still not installed.
Today I hit the button and reset my controller.
After this it now shows me as "Owner connected" and I can raise the line current and phase current values again.
The controller has kept all his values except pole pairs and motor temperature sensor and upper and low voltage level.

But now the controller is stuck in Auto Learn and does not turn the motor anymore.
I have done the Auto Learn with 5 different Fardriver and never had any problem with it.
Anyone got a hint, what I'm probably doing wrong?

Screenshot_20260702_212105.jpgScreenshot_20260702_212044.jpgScreenshot_20260702_212036.jpgScreenshot_20260702_212032.jpg
 
Last edited:
After trying a few different firmwares the controller has finished Auto Learn and I can now drive again.

Actually I can't activate regeneration and can't change regen current.
But I changed current to 450/1600A.
When I change the BMS, I will try more line amps.
 
Last edited:
New measurements 0-100kph with 450bA and 1600pA
With the new 30p BMS I will shure get under 6 seconds.
These dips in the acceleration graph of the 10Hz GPS are not present on the road, they must be slightly off measurements as you can't see any bigger current reductions in the fardriver graph.
Screenshot_20260706_063626.jpg
Screenshot_20260706_062005_GNSS PA.jpg

When the BMS is changed the battery current can be raised to 500A.
From there on it is time to loose some weight to get faster.
 
Last edited:
Hi Dominik, what kind of BMS are you using. In the moment I like the jk BMS. But they are more or less limited to 24s. Searching for one with 28s. Thanks
 
I have used the JK-B2A-24S-20P HC and will change to the new 30P Version.
As I have bricked my Fardriver ND721800, I have ordered a new ND841800 and if I ever need a new battery this will be built with 2 VW 12S MEB modules with 2x6,85kWh.
Easiest way to get a good and small battery, that will give me 450-500A and it fits perfectly in my scooter leaving enough space for a 8kW charger or even more.

JK offers a 32S 300A Relais BMS which is big compared to the a 32S 150A 15P BMS
32S 150A BMS
32S 300A Relais BMS
 
Last edited:
New Controller arrived. ND841800
But the CAN Version, missing all the small plugs my three other Fardrivers have. It has only two big 9 pin plugs and hall and Bluetooth.
IMG-20260807-WA0004.jpeg

It came without a wiring diagram and without stickers on the wires.


I bricked my old one with a wrong firmware.
Will dissamble my old one and probably I will find someone who puts a VESC Controll board inside.
 
New ND841800 ist installed but it is limiting phase current to 700A, even when I set it to 1800A

Any hints what might be wrong?

0-100kph times are slower and acceleration feels slugish, I only hit 0.5g before it was 0.7-0.8g

Screenshot_20260816_140753_dragy.jpg

Overall power is ok still seeing more than 32kW.
When the battery current limit is reached acceleration feels exactly the same as with the 721800.
At the end of the run there was a curve, i had to slow down.
Screenshot_20260816_141617_dragy.jpg
 
Back