auraslip
10 MW
- Joined
- Mar 5, 2010
- Messages
- 3,535


Ok, these packs have ~200 cycles at 5c max 1.5c normal. Charged to 4.15v - discharged no lower than 3v and typically to 70% DOD. Never abused to my knowledge.
I pulled these out of my bike with it's enclosed battery box after riding for 6 months. I DID NOT NOTICE IT WAS PUFFED UNTIL THE NEXT DAY. So either it was puffed and I didn't see it until I went to unwrap the tape wrap, or I did something to it when I put it in the storage closet that caused it to puff. At first I was thinking I was 99% sure it wasn't puffed when I took it out, but now I'm only 50% sure.
Battery was removed at ~4v. All cells still roughly balanced at ~4v
What to do with it?
Also, I'm gonna do a capacity test on the 7 other non-puffed 4s packs in the next few days. I'll post info in here.
fyi pack is 22s10ah with 4s packs and 6s packs.