ice_robin said:NMC may means Li-Ni-Co-Mn, but I still thinks lifepo4 is better, it is more stable.
liveforphysics said:ice_robin said:NMC may means Li-Ni-Co-Mn, but I still thinks lifepo4 is better, it is more stable.
In GM's 50Million dollar cell testing program for the Chev Volt batteries, LG Chem's NMC cells won out over A123 LiFePO4 cells because of the increased safety and stability of NMC.
Our 14S 9P, 50V 18.5Ah Samsung SDI Battery Pack uses the SDI ICR18650-22P 4.5C rated cell.
Discharge curves at 2,3, & 5A ...
http://www.dampfakkus.de/akkutest.php?id=73
wb9k said:liveforphysics said:ice_robin said:NMC may means Li-Ni-Co-Mn, but I still thinks lifepo4 is better, it is more stable.
In GM's 50Million dollar cell testing program for the Chev Volt batteries, LG Chem's NMC cells won out over A123 LiFePO4 cells because of the increased safety and stability of NMC.
I what ways are they safer or more stable? And why would GM use A123 cells for the Spark if the Volt's cells are superior? I heard a different story about why A123 wasn't in the Volt, and while I can't say for sure if it's true, it's very plausible in the context visible from my perspective.
LFP has been putting out misinformation about batteries ever since I have been reading this forum.
He is for sure the worst guru on our forum.
He bragged up using hk lipo for a long time and when I was a newbee I bought some.
Worst batteries I ever bought and wasted money.
I should have never read any of his posts.
He is bad for the ebike movement. A total joker that does not help people understand but confuses people.
nicobie said:LFP has been putting out misinformation about batteries ever since I have been reading this forum.
He is for sure the worst guru on our forum.
He bragged up using hk lipo for a long time and when I was a newbee I bought some.
Worst batteries I ever bought and wasted money.
I should have never read any of his posts.
He is bad for the ebike movement. A total joker that does not help people understand but confuses people.
Maybe you should inform Zero motorcycles of your opinion. He is their battery expert. He also did the same thing for Microsoft.
I am interested in your qualifications as a battery expert. But until you can prove that you know more that LFP, I suggest that you keep your mouth shut. You really do come off as a total idiot.
I look at you as just another opinionated fool with not much experience.
Ever heard of the "signal to noise ratio"? Your posts are the noise part.
Have a nice day![]()
SamTexas said:http://em3ev.com/store/index.php?route=product/product&path=35&product_id=123
The above link is a shameless, deliberate lie. In their own words:
Our 14S 9P, 50V 18.5Ah Samsung SDI Battery Pack uses the SDI ICR18650-22P 4.5C rated cell.
Samsung ICR18650-22P is NOT NMC. ICR = Lithium (I) Cobalt (C) Rechargeable (R). Real life test have shown that this cell can barely tolerate 5A (2.27C) continuous discharge, let alone 9.9A (4.5C) as claimed by the seller.